Model No: Ti 40

AMS 4902/UNS R50400/W.Nr 3.7035/Ti 40 Titanium Alloy Strip

Ti 40 titanium alloy the two most useful properties of the metal are corrosion resistance and strength-to-density ratio, the highest of any metallic element. The corrosion resistance of Ti 40 titanium alloy at normal temperatures is unusually high.
Delivery :
FOB
minimum order :
100 kilograms
Supply Ability :
5000Tonkilograms / Month
Stock Time :
7-10Day
Country of Origin :
CHINA
Quantity :
Contact Now
Titanium's unique combination of physical, mechanical and corrosion resistant properties makes it an ideal material for many different applications. Titanium's high strength to weight ratio makes titanium the prime choice for high strength, lightweight applications.
 
Titanium alloys the two most useful properties of the metal are corrosion resistance and strength-to-density ratio, the highest of any metallic element. The corrosion resistance of titanium alloys at normal temperatures is unusually high. These properties determine the application of titanium and its alloys.

UNS R50400/W.Nr 3.7035/Ti 40 Titanium Alloy Strip Applications

Aircraft skins and equipment, marine and chemical equipment, and cryogenic vessels.

Description

CP Titanium alloy grade 2 combines excellent formability and moderate strength with superior corrosion resistance.

Industries Supplied

  • Power Generation
  • Chemical Processing
  • Aerospace
  • Medical

Nominal Composition

Fe: 0.30 max
O: 0.20 max
C: 0.08 max
N: 0.05 max
H: 0.0150 max
Ti: Balance

Physical Properties

Density: 0.163 lb/in3, (4.51 g/cm3)
Modulus of Elasticity (E):
At 70°F (20°C): 16.3 x 103 ksi (112 GPa)
Modulus of Rigidity (G)
At 70°F (20°C): 5.9 x 103 ksi (41 GPa)
Coefficient of Expansion:
5.4 µin/in.-°F (70°F to 932°F)
9.7 µm/m-°C (20°C to 500°C)
Electrical Resistivity: 21 µΩ.in, (53.3 µΩ.cm)
Thermal Conductivity: 12.6 Btu-in/ft2hr-°F, (21.79 W/m-K)

Applicable Specifications

Strip and Foil: AMS 4902, ASTM B265

UNS R50400/W.Nr 3.7035/Ti 40 Titanium Alloy Typical Mechanical Properties

Annealed
Heat Treatment: 1290°F
Tensile Strength: 70 ksi (485 MPa)
Suggested Operating Conditions: -300°F to 1000°F (-184°C to 540°C)