ASTM F562 / UNS R30035 / 35N LT Cobalt Superalloy

ASTM F562 35N LT is a cobalt-base superalloy produced by a melt practice that results in improved fatigue life for wires used in the medical field. 35N LT alloy provides an excellent combination of strength, fatigue resistance, corrosion resistance, and good biocompatibility.
Delivery :
FOB
minimum order :
100 kilograms
Supply Ability :
5000Tonkilograms / Month
Stock Time :
7-10Day
Country of Origin :
CHINA
Quantity :
Contact Now
ASTM F562 35N LT is a cobalt-base superalloy produced by a melt practice that results in improved fatigue life for wires used in the medical field. 35N LT alloy provides an excellent combination of strength, fatigue resistance, corrosion resistance, and good biocompatibility.
 
35N LT and Nitinol are biomedically significant materials used in implantable medical devices requiring high fatigue resistance.

Chemical composition

CompositionASTM F562
UNS R30035 %
Carbon0.025 max
Manganese0.15 max
Silicon0.15 max
Phosphorus0.015 max
Sulfur0.010 max
Chromium19.0 - 21.0
Nickel33.0 - 37.0
Molybdenum9.0 - 10.5
Iron1.0 max
Titanium0.01 max
Boron0.015 max
CobaltBalance

Physical properties

MetricEnglish
Density8.41 g/cm³0.304 lbs/in³
Modulus of elasticity233 Gpa33.8 Mpsi
Electrical resistivity1033 µohm*mm40.7 µohm*in
Thermal conductivity11.2 W/(m*°C)77.7 BTU*in/(hr*ft²*°F)
Coefficient of thermal
expansion
12.8 µm/(m*°C)7.11 µin/(in*°F)

*Values calculated at 22 °C [72 °F]

Mechanical properties

Cold worked
%
Yield strengthUltimate tensile strengthElongation %
0896 MPa [130 ksi]1310 MPa [190 ksi]33
201310 MPa [190 ksi]1650 MPa [240 ksi]6.4
371650 MPa [240 ksi]1930 MPa [280 ksi]3.9

50

1860 MPa [270 ksi]2070 MPa [300 ksi]3.5

60

2000 MPa [290 ksi]2210 MPa [320 ksi]3.5

68

2070 MPa [300 ksi]2280 Mpa [330 ksi]2.6

75

2100 MPa [305 ksi]2340 MPa [340 ksi]2.5

80

2170 MPa [315 ksi]2410 MPa [350 ksi]2.3

84

2240 MPa [325 ksi]2480 MPa [360 ksi]2.8

90

2300 MPa [333 ksi]2550 MPa [370 ksi]2.4

93

2330 MPa [338 ksi]2590 MPa [375 ksi]2.3

* Values are typical and may not represent all diameters. Test method will affect results.
All data represent results from a 25.4 cm [10 in] test gauge length.

 
Lork Group is a metal material manufacturer and exporter in China
 
The experts at Lork Group are ready to help you choose the most suitable type of Metal.
 
We have built a reputation as a trusted partner for quality materials, distributing numerous grades of stainless steel, nickel alloy, Precision Alloy, and hard-to-find metals. Our raw metal bars, rings, plates, pipes, and tubing are available from stock.
 
To learn more about the Lork Group metal difference and our stainless steel and super alloy material offerings, contact us or request a quote today.