Subscribe to our Newsletter
Model No: 8CrSi7-7
8CrSi7-7
8CrSi7-7 steel, German DIN standard heat-resistant steel.
Delivery :
FOB
minimum order :
100 kilograms
Supply Ability :
5000Tonkilograms / Month
Stock Time :
7-10Day
Country of Origin :
CHINA
Quantity :
8CrSi7-7 Description
8CrSi7-7 steel, German DIN standard heat-resistant steel.
Chemical composition(mass fraction)(wt.%) of the 8CrSi7-7
| C(%) | Si(%) | Mn(%) | P(%) | s(%) | Cr(%) |
| Max 0.10 | 1.50-1.80 | Max 1.00 | Max 0.045 | Max 0.030 | 1.50-2.00 |
Mechanical Properties of steel grade 8CrSi7-7
| Yield Ro.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku () | Elongation A (%) | Reduction in cross section on fracture Z(%) | As-Heat-Treated Condition | Brinell hardness (HBW) |
| 271(≥) | 769 [≥] | 44 | 41 | 41 | Solution and Aging. Annealing,Ausaging. Q+T.etc | 231 |
Physical Properties of steel grade 8CrSi7-7
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coeffcient of thermal expansion 10- 6/(°C)between 20(°c) and | Thermal conductivity (W/m.°C) | Specifc thermal capacity (/kg·°c) | Specifc electrical resistivity (2 mm'/m) | Density (kg/dm³) | Poisson's coeffcient, L |
| 14 | - | - | 0.11 | - | - | ||
| 484 | 287 | - | 22.3 | 133 | - | - | - |
| 162 | - | 11 | 44.2 | - | - | 214 | 343 |