Subscribe to our Newsletter
Model No: Hastelloy C4
Hastelloy C4
Hastelloy C4 is a Nickel-Chromium-Molybdenum alloy that offers exceptional stabilization at the elevated temperatures, good ductility and resistance to corrosion properties.
Delivery :
FOB
minimum order :
100 kilograms
Supply Ability :
5000Tonkilograms / Month
Stock Time :
7-10Day
Country of Origin :
CHINA
Quantity :
Hastelloy C4 Description
Hastelloy C4 is a Nickel-Chromium-Molybdenum alloy that offers exceptional stabilization at the elevated temperatures, good ductility and resistance to corrosion properties. It retains its characteristics even after aging up to 1200oF to 1900oF or 649oC to 1038oC. Hastelloy C4 offers resistance to grain development precipitation in the welding area so it is highly suitable for the chemical processes in the welding condition. It offers extremely high resistance to stress corrosion cracking and oxidizing conditions up to 1900oF or 1038oC.
Hastelloy C4 offers resistance to mineral acids, organic and inorganic acids, sea water and brine solutions. It has service temperature up to 1900oF or 1038oC. Outstanding resistance to high temperature corrosion and stress corrosion cracking. Great material for use in chemical processing plants and nuclear fuel processing.
Hastelloy C4 Other Designations
Other designations that are equivalent to Hastelloy(r) C-4 include:
ASTM B574
ASTM B575
ASTM B619
ASTM B622
ASTM B626
DIN 2.4610
Hastelloy C4 Chemical Composition
The chemical composition of Hastelloy C4 is outlined in the following table.
| Element | Content (%) |
| Chromium, Cr | 14-18 |
| Molybdenum, Mo | 14-17 |
| Iron, Fe | 3 max |
| Cobalt, Co | 2 max |
| Manganese, Mn | 1 max |
| Titanium, Ti | 0.7 max |
| Silicon, Si | 0.08 max |
| Phosphorus, P | 0.04 max |
| Sulfur, S | 0.03 max |
| Carbon, C | 0.015 max |
| Nickel, Ni | Remainder |
Mechanical Properties
The mechanical properties of Hastelloy C4 are outlined in the following table.
| Properties | Metric | Imperial |
| Tensile strength | 738 MPa | 107000 psi |
| Yield strength ( @ 0.2% offset) | 492 MPa | 71400 psi |
| Elastic modulus | 211 GPa | 30600 ksi |
| Elongation at break (in 50.8 mm) | 42% | 42% |
Machinability
Hastelloy C4 can be machined using conventional methods.
Forming
Hastelloy C4 can be easily formed using conventional techniques.
Welding
Except submerged arc and oxy-acetylene welding methods, Hastelloy (r ) C4 can be welded using all other welding methods.
Heat Treatment
Hastelloy C4 is heat treated by annealing at 1066°C (1950°F) followed by quenching.
Forging
Hastelloy C4 is hot forged at 955 to 1177°C (1750 to 2150°F).
Hot Working
Hastelloy C4 is hot extruded or hot worked similar to that of stainless steels.
Cold Working
Hastelloy C4 can be cold worked using conventional methods.
Annealing
Hastelloy C4 is annealed at 1066°C (1950°F) followed by quenching.
Aging
Hastelloy C4 is aged at 649°C (1200°F) for 10 h in order to improve its yield strength and ductility without decreasing its ultimate tensile strength.
Hardening
Hastelloy C4 is hardened by cold working.
Hastelloy C4 Applications
Chemical processing equipment
Nuclear fuel processing
Lork Group is an supplier of industrial metals to the global aerospace, oil and gas, power generation, petrochemical, bio-medical, pharmaceutical, and other high tech manufacturing industries. Products of premium metal products including Inconel alloys,Incoloy alloys,Monel alloys,Haynes alloys,Hastelloy alloy,stainless steelandother superalloy. We certify to most ASME, ASTM, AMS, and military specifications as well as most international standards certification.